{"title":"DC--11 Inserts","description":"\u003cp\u003e\u003cstrong\u003eDC--11 Inserts\u003c\/strong\u003e are 55° positive turning inserts (DCGT\/DCMT) designed for repeatable lathe machining with consistent geometry. They are used for finishing and semi-roughing, helping control chip evacuation and achieve stable surface quality across demanding cutting conditions.\u003c\/p\u003e\u003cp\u003eAvailable with multiple chipbreaker geometries, carbide grades and PVD\/CVD coatings, plus options tailored to steel, stainless, cast iron and non-ferrous materials. Choose suitable combinations from \u003cstrong\u003eYg\u003c\/strong\u003e \u0026 \u003cstrong\u003eEchain\u003c\/strong\u003e based on your workpiece and cutting parameters.\u003c\/p\u003e\u003cp\u003eConsider feed, depth of cut, coolant strategy and toolholder rigidity to maximize tool life, reduce vibration and keep dimensional accuracy under control.\u003c\/p\u003e","products":[{"product_id":"dcmw11t3-ha-plakidia-dcmw11t3-ha-gia-mantemi-kai-bammena","title":"Inserts - DCMW11T3**-HA for Cast Iron and Painted Surfaces","description":"\u003ch3\u003eMachining Materials\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(K)\u003c\/em\u003e\u003c\/strong\u003e - Cast Irons - Grey Cast Iron (Cast Iron)\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(H)\u003c\/em\u003e\u003c\/strong\u003e - Hardened Materials - Painted (Hardened Steel)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eChipbreaker\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(..MA)\u003c\/em\u003e\u003c\/strong\u003e - Designed for machining brittle materials such as cast irons and painted steels. It has no geometry on the cutting edge. Suitable for heavy roughing **\u003cem\u003e\u003cem\u003e(\u003c\/em\u003eroughing\u003c\/em\u003e) in cast irons and light machining in painted steels.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eLathe inserts from Dormer Pramet\u003c\/strong\u003e, a leading cutting tool manufacturer.\nThe choice of the appropriate insert depends on the \u003cstrong\u003echipbreaker\u003c\/strong\u003e, i.e., the geometry that helps in breaking and removing the chip, as well as the \u003cstrong\u003egrade\u003c\/strong\u003e, which describes the microstructure and coating of the insert and directly affects hardness and fracture toughness. The \u003cstrong\u003ecutting conditions\u003c\/strong\u003e (speed, feed, depth) must be carefully defined to achieve maximum tool performance and life.\u003c\/p\u003e","brand":"Pramet","offers":[{"title":"11 \/ Painted - Cast Iron \/ 0.4","offer_id":52638117527875,"sku":"DCMW11T304-HA","price":9.6,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0572\/8396\/9077\/files\/DCMW07-HA_-_07mm_fa024609-6ebb-4425-83ea-b50aa1a23c18.png?v=1740399415"},{"product_id":"dcmt11t3-jo-plakidia-dcmt11t3-jo-gia-atsali","title":"Inserts - DCMT11T3**-JO for Steel","description":"\u003ch3\u003eMachining Materials\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P)\u003c\/em\u003e\u003c\/strong\u003e - Steels - Alloy Steels (Steel - Alloy Steel)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eEconomical lathe inserts from Echain\u003c\/strong\u003e, a cutting tool manufacturer from Taiwan.\nThe choice of the appropriate insert depends on the \u003cstrong\u003echipbreaker\u003c\/strong\u003e, that is the geometry that helps in breaking and removing the waste, as well as on the \u003cstrong\u003egrade\u003c\/strong\u003e, which describes the microstructure and coating of the insert and directly affects hardness and brittleness. The \u003cstrong\u003ecutting conditions\u003c\/strong\u003e (speed, feed, depth) must be carefully set to achieve maximum tool performance and lifespan.\u003c\/p\u003e","brand":"Echain","offers":[{"title":"11 \/ 0.8 \/ ECP200","offer_id":52638149935427,"sku":"DCMT11T308-JO","price":5.5,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0572\/8396\/9077\/files\/DCMT070204-UG_YG3115.png?v=1740399982"},{"product_id":"dcgt11t3-sf-plakidia-dcgt11t3-sf-gia-yperkramata","title":"DCGT11T3**-SF Inserts for Superalloys","description":"\u003ch3\u003eWorkpiece Materials\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(S)\u003c\/em\u003e\u003c\/strong\u003e - High-temperature Superalloys (Fe,Ni,Co) - Titanium Alloys (HRSA, Titanium alloys)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eChipbreaker\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(SF)\u003c\/em\u003e\u003c\/strong\u003e - Geometry specially designed for finishing machining of superalloys and titanium alloys. Features a \u003cstrong\u003elarge rake angle\u003c\/strong\u003e (\u003cem\u003erake angle\u003c\/em\u003e) with a short length and is available with \u003cstrong\u003esmall cutting radii\u003c\/strong\u003e (\u003cem\u003eRE\u003c\/em\u003e). Suitable for small cutting depths (\u003cem\u003eAp\u003c\/em\u003e) and low feeds (\u003cem\u003eFn\u003c\/em\u003e). Ensures excellent surface quality.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eGrade\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eYG401\u003c\/em\u003e\u003c\/strong\u003e – For superalloys (HRSA) (S10–S20). Durable PVD TiAlSiN coating for excellent protection and lubrication.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eFeed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eFn\u003c\/em\u003e\u003c\/strong\u003e = 0.03~0.20 mm\/rev\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eCutting Speed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(S31-37)\u003c\/em\u003e\u003c\/strong\u003e - Vc=30~90 m\/min\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eTurning inserts from YG1\u003c\/strong\u003e, a leading cutting tool manufacturer from Korea.\nThe choice of the appropriate insert depends on the \u003cstrong\u003echipbreaker\u003c\/strong\u003e, that is, the geometry that helps in breaking and removing the chip, as well as the \u003cstrong\u003egrade\u003c\/strong\u003e, which describes the microstructure and coating of the insert and directly affects hardness and fracture toughness. The \u003cstrong\u003ecutting conditions\u003c\/strong\u003e (speed, feed, depth) must be carefully defined to achieve maximum tool performance and life.\u003c\/p\u003e","brand":"Yg","offers":[{"title":"0.10~2.5 \/ 0.1 \/ YG401","offer_id":53063598670147,"sku":"DCGT11T301-SF-YG401","price":8.5,"currency_code":"EUR","in_stock":true},{"title":"0.10~2.5 \/ 0.2 \/ YG401","offer_id":53063598735683,"sku":"DCGT11T302-SF-YG401","price":8.5,"currency_code":"EUR","in_stock":true},{"title":"0.10~2.5 \/ 0.4 \/ YG401","offer_id":53063598702915,"sku":"DCMT11T304-SF-YG401","price":6.5,"currency_code":"EUR","in_stock":true},{"title":"0.10~2.5 \/ 0.8 \/ YG401","offer_id":53063598768451,"sku":"DCGT11T308-SF-YG401","price":8.5,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0572\/8396\/9077\/files\/DCGT11T302-SF_e6bf2960-0ecd-4697-9e3f-4f30a353b8fc.png?v=1740401369"},{"product_id":"dcmt11t3-uf-plakidia-dcmt11t3-uf-gia-atsalia-finirisma","title":"DCMT11T3**-UF Inserts for Steels - Finishing","description":"\u003ch3\u003eMachining Materials\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P)\u003c\/em\u003e\u003c\/strong\u003e - Steels - Alloy Steels (Steel - Alloy Steel)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eChipbreaker\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(UF)\u003c\/em\u003e\u003c\/strong\u003e - Geometry specially designed for finishing on steels. It features a \u003cstrong\u003esmall rake angle\u003c\/strong\u003e (\u003cem\u003erake angle\u003c\/em\u003e) and is available with \u003cstrong\u003esmall cutting radii\u003c\/strong\u003e (\u003cem\u003eRE\u003c\/em\u003e). Suitable for small cutting depths (\u003cem\u003eAp\u003c\/em\u003e) and low feeds (\u003cem\u003eFn\u003c\/em\u003e). Ensures excellent surface quality.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eGrade\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eYG3115\u003c\/em\u003e\u003c\/strong\u003e – New grade for high machining speeds on steels (P15–P25). CVD MT-TiCN–Al₂O₃ coating. Ideal for mass production with stable tool life and minimization of built-up edge formation.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eFeed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eFn\u003c\/em\u003e\u003c\/strong\u003e = 0.05~0.25 mm\/rev\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eCutting Speed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P1-5)\u003c\/em\u003e\u003c\/strong\u003e - Vc=180~500 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P5-9)\u003c\/em\u003e\u003c\/strong\u003e - Vc=170~450 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P10-11)\u003c\/em\u003e\u003c\/strong\u003e - Vc=60~300 m\/min\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eTurning inserts from YG1\u003c\/strong\u003e, a leading cutting tool manufacturer from Korea.\nThe choice of the appropriate insert depends on the \u003cstrong\u003echipbreaker\u003c\/strong\u003e, that is, the geometry that helps in breaking and removing the chip, as well as on the \u003cstrong\u003egrade\u003c\/strong\u003e, which describes the microstructure and coating of the insert and directly affects hardness and fracture toughness. The \u003cstrong\u003ecutting conditions\u003c\/strong\u003e (speed, feed, depth) must be carefully defined to achieve maximum performance and tool life.\u003c\/p\u003e","brand":"Yg","offers":[{"title":"0.50~2.0 \/ 0.4 \/ YG3115","offer_id":52950533243203,"sku":"DCMT11T304-UF-YG3115","price":6.5,"currency_code":"EUR","in_stock":true},{"title":"1.00~2.0 \/ 0.8 \/ YG3115","offer_id":52950533275971,"sku":"DCMT11T308-UF-YG3115","price":6.5,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0572\/8396\/9077\/files\/DCMT070204-UF_YG3115_972791a8-83ce-4b70-b1e5-494d7cf005f8.png?v=1740401496"},{"product_id":"dcgt11t3-al-plakidia-dcgt11t3-al-gia-alouminio","title":"DCGT11T3**-AL Inserts for Aluminum","description":"\u003ch3\u003eMachining Materials\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(N)\u003c\/em\u003e\u003c\/strong\u003e - Non-ferrous materials - Aluminum, Copper alloys, Plastic (Aluminum, Copper alloys, non metallic materials)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eChipbreaker\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(AL)\u003c\/em\u003e\u003c\/strong\u003e - Geometry for general machining of aluminum and non-metallic materials. Features a \u003cstrong\u003eparticularly large rake angle\u003c\/strong\u003e (\u003cem\u003erake angle\u003c\/em\u003e) for smoother chip flow and to avoid built-up edge due to material adhesion on the cutting edge. Suitable for moderate machining of soft (sticky) materials.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eGrade\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eYG10\u003c\/em\u003e\u003c\/strong\u003e – Uncoated for general aluminum machining (N05–N25). Very smooth surface to minimize built-up edge formation.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eFeed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eFn\u003c\/em\u003e\u003c\/strong\u003e = 0.02~0.30 mm\/rev\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eCutting Speed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(N21-30)\u003c\/em\u003e\u003c\/strong\u003e - Vc=250~800 m\/min\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eTurning inserts from YG1\u003c\/strong\u003e, a leading cutting tool manufacturer from Korea.\nThe choice of the appropriate insert depends on the \u003cstrong\u003echipbreaker\u003c\/strong\u003e, i.e., the geometry that helps in breaking and removing the chip, as well as the \u003cstrong\u003egrade\u003c\/strong\u003e, which describes the microstructure and coating of the insert and directly affects hardness and fracture toughness. The \u003cstrong\u003ecutting conditions\u003c\/strong\u003e (speed, feed, depth) must be carefully set to achieve maximum tool performance and life.\u003c\/p\u003e","brand":"Yg","offers":[{"title":"0.05~4.0 \/ 0.1 \/ YG10","offer_id":52950532063555,"sku":"DCGT11T301-AL","price":7.1,"currency_code":"EUR","in_stock":true},{"title":"0.05~4.0 \/ 0.2 \/ YG10","offer_id":52950532129091,"sku":"DCGT11T302-AL","price":7.1,"currency_code":"EUR","in_stock":true},{"title":"0.10~5.0 \/ 0.4 \/ YG10","offer_id":52950532096323,"sku":"DCGT11T304-AL","price":7.1,"currency_code":"EUR","in_stock":true},{"title":"1.00~5.0 \/ 0.8 \/ YG10","offer_id":52950532161859,"sku":"DCGT11T308-AL","price":7.1,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0572\/8396\/9077\/files\/DCGT070204-AL_3418f3ae-fb65-4701-8bdc-f5cf2d2a391e.png?v=1740402262"},{"product_id":"dcmt11t3-ug-plakidia-dcmt11t3-ug-gia-atsalia-genikh","title":"DCMT11T3**-UG Inserts for Steels - General Machining","description":"\u003ch3\u003eProcessing Materials\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P)\u003c\/em\u003e\u003c\/strong\u003e - Steels - Alloy Steels (Steel - Alloy Steel)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eChipbreaker\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(UG)\u003c\/em\u003e\u003c\/strong\u003e - Geometry for general processing of steels. It features a relatively \u003cstrong\u003elarge rake angle\u003c\/strong\u003e (\u003cem\u003erake angle\u003c\/em\u003e) for smoother chip flow and a \u003cstrong\u003ereinforced cutting edge\u003c\/strong\u003e with a flat section on the edge (\u003cem\u003eT-land\u003c\/em\u003e). Suitable for medium machining and continuous cutting. Combines \u003cstrong\u003etoughness\u003c\/strong\u003e (\u003cem\u003etoughness\u003c\/em\u003e) and \u003cstrong\u003ehigh wear resistance\u003c\/strong\u003e (\u003cem\u003ewear resistance\u003c\/em\u003e)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eGrade\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eYG3020\u003c\/em\u003e\u003c\/strong\u003e – First choice for general steel machining (P15–P30). CVD TiCN–Al₂O₃ coating. Substrate specially designed for high toughness and smooth surface for increased wear resistance.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eFeed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eFn\u003c\/em\u003e\u003c\/strong\u003e = 0.15~0.30 mm\/rev\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eCutting Speed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P1-5)\u003c\/em\u003e\u003c\/strong\u003e - Vc=160~380 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P5-9)\u003c\/em\u003e\u003c\/strong\u003e - Vc=140~320 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P10-11)\u003c\/em\u003e\u003c\/strong\u003e - Vc=60~130 m\/min\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eTurning inserts from YG1\u003c\/strong\u003e, a top cutting tool manufacturer from Korea.\nThe choice of the appropriate insert depends on the \u003cstrong\u003echipbreaker\u003c\/strong\u003e, that is the geometry that helps in breaking and removing the chip, as well as the \u003cstrong\u003egrade\u003c\/strong\u003e, which describes the microstructure and coating of the insert and directly affects hardness and toughness. The \u003cstrong\u003ecutting conditions\u003c\/strong\u003e (speed, feed, depth) must be carefully set to achieve maximum tool performance and life.\u003c\/p\u003e","brand":"Yg","offers":[{"title":"0.50~2.5 \/ 0.4 \/ YG3125","offer_id":52950533308739,"sku":"DCMT11T304-UG-YG3125","price":6.5,"currency_code":"EUR","in_stock":true},{"title":"0.80~2.5 \/ 0.8 \/ YG3125","offer_id":53221446287683,"sku":"DCMT11T308-UG-YG3125","price":6.5,"currency_code":"EUR","in_stock":true},{"title":"1.50~3.0 \/ 1.2 \/ YG3125","offer_id":52950533374275,"sku":"DCMT11T312-UG-YG3125","price":6.5,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0572\/8396\/9077\/files\/DCMT070204-UG_YG3115_f2924f5e-7943-45f5-9280-1eaa68a51bc9.png?v=1740402325"},{"product_id":"dcmt11t3-mf-plakidia-dcmt11t3-mf-gia-inox-finirisma","title":"DCMT11T3**-MF Inserts for Stainless Steel - Finishing","description":"\u003ch3\u003eWorkpiece Materials\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(M)\u003c\/em\u003e\u003c\/strong\u003e - Stainless Steels (Stainless Steel - Inox)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eChipbreaker\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(MF)\u003c\/em\u003e\u003c\/strong\u003e - Geometry specially designed for finishing stainless steels. It features a \u003cstrong\u003eparticularly small rake angle\u003c\/strong\u003e (\u003cem\u003erake angle\u003c\/em\u003e) and is available with relatively \u003cstrong\u003esmall cutting radii\u003c\/strong\u003e (\u003cem\u003eRE\u003c\/em\u003e). Suitable for small cutting depths (\u003cem\u003eAp\u003c\/em\u003e) and low feeds (\u003cem\u003eFn\u003c\/em\u003e). Ensures excellent surface quality.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eGrade\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eYG211\u003c\/em\u003e\u003c\/strong\u003e – First choice for finishing stainless steels (M05–M25). PVD TiAlN coating for excellent wear resistance.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eFeed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eFn\u003c\/em\u003e\u003c\/strong\u003e = 0.06~0.25 mm\/rev\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eCutting Speed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(M12-13)\u003c\/em\u003e\u003c\/strong\u003e - Vc=170~270 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(M14)\u003c\/em\u003e\u003c\/strong\u003e - Vc=150~230 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(S31-37)\u003c\/em\u003e\u003c\/strong\u003e - Vc=30~100 m\/min\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eTurning inserts from YG1\u003c\/strong\u003e, a top cutting tool manufacturer from Korea.\nThe choice of the appropriate insert depends on the \u003cstrong\u003echipbreaker\u003c\/strong\u003e, that is the geometry that helps in breaking and removing the chip, as well as on the \u003cstrong\u003egrade\u003c\/strong\u003e, which describes the microstructure and coating of the insert and directly affects hardness and fracture toughness. The \u003cstrong\u003ecutting conditions\u003c\/strong\u003e (speed, feed, depth) must be carefully set to achieve maximum tool performance and life.\u003c\/p\u003e","brand":"Yg","offers":[{"title":"0.10~2.0 \/ 0.4 \/ YG211","offer_id":52950532882755,"sku":"DCMT11T304-MF-YG211","price":6.5,"currency_code":"EUR","in_stock":true},{"title":"0.08~2.0 \/ 0.2 \/ YG211","offer_id":52950532915523,"sku":"DCMT11T302-MF-YG211","price":6.5,"currency_code":"EUR","in_stock":true},{"title":"0.15~2.0 \/ 0.8 \/ YG211","offer_id":52950532948291,"sku":"DCMT11T308-MF-YG211","price":6.5,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0572\/8396\/9077\/files\/DCMT11T308-MF_70bb3be1-58e2-4589-8fd7-402536513929.png?v=1740402354"},{"product_id":"dcmt11t3-mm-plakidia-dcmt11t3-mm-gia-atsalia-kai-inox","title":"DCMT11T3**-MM Inserts for Steel and Stainless Steel - General Use","description":"\u003ch3\u003eMachining Materials\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(M)\u003c\/em\u003e\u003c\/strong\u003e - Stainless Steels (Stainless Steel - Inox)\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P)\u003c\/em\u003e\u003c\/strong\u003e - Steels - Alloy Steels (Steel - Alloy Steel)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eChipbreaker\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(MM)\u003c\/em\u003e\u003c\/strong\u003e - Geometry for general machining of stainless steels. It features a relatively \u003cstrong\u003elarge rake angle\u003c\/strong\u003e (\u003cem\u003erake angle\u003c\/em\u003e) for smoother chip flow and a \u003cstrong\u003ereinforced cutting edge\u003c\/strong\u003e with a flat section on the edge (\u003cem\u003eT-land\u003c\/em\u003e). Suitable for medium machining on stainless steel and steel. Combines \u003cstrong\u003etoughness\u003c\/strong\u003e (\u003cem\u003etoughness\u003c\/em\u003e) and \u003cstrong\u003ehigh wear resistance\u003c\/strong\u003e (\u003cem\u003ewear resistance\u003c\/em\u003e)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eGrade\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eYG2025\u003c\/em\u003e\u003c\/strong\u003e – New CVD grade for stainless steels with high speed (M15–M35). New CVD TiCN - Al₂O₃ coating technology. Combination of new substrate and coating for excellent wear resistance and minimization of built-up edge formation. Also works excellently on steels - alloy steels (ISO P group)\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eFeed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eFn\u003c\/em\u003e\u003c\/strong\u003e = 0.08~0.25 mm\/rev\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eCutting Speed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P1-5)\u003c\/em\u003e\u003c\/strong\u003e - Vc=120~220 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P5-9)\u003c\/em\u003e\u003c\/strong\u003e - Vc=120~200 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(M12-13)\u003c\/em\u003e\u003c\/strong\u003e - Vc=170~220 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(M14)\u003c\/em\u003e\u003c\/strong\u003e - Vc=150~200 m\/min\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eTurning inserts from YG1\u003c\/strong\u003e, a top cutting tool manufacturer from Korea.\nThe choice of the appropriate insert depends on the \u003cstrong\u003echipbreaker\u003c\/strong\u003e, that is the geometry that helps in breaking and removing the chip, as well as on the \u003cstrong\u003egrade\u003c\/strong\u003e, which describes the microstructure and coating of the insert and directly affects hardness and toughness. The \u003cstrong\u003ecutting conditions\u003c\/strong\u003e (speed, feed, depth) must be carefully set to achieve maximum tool performance and life.\u003c\/p\u003e","brand":"Yg","offers":[{"title":"0.25~3.0 \/ 0.4 \/ YG2025","offer_id":52950533046595,"sku":"DCMT11T304-MM-YG2025","price":6.5,"currency_code":"EUR","in_stock":true},{"title":"0.40~3.0 \/ 0.8 \/ YG2025","offer_id":53772201394499,"sku":"DCMT11T308-MM-YG2025","price":6.5,"currency_code":"EUR","in_stock":true},{"title":"0.50~3.0 \/ 1.2 \/ YG2025","offer_id":52950533013827,"sku":"DCMT11T312-MM-YG2025","price":6.5,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0572\/8396\/9077\/files\/DCMT11T308-MM_2d312382-3236-46d4-a5d5-d01e6d8182dd.png?v=1740402384"},{"product_id":"dcmt11t3-pf-plakidia-dcmt11t3-pf-cermet-gia-atsalia-mantemi","title":"DCMT11T3**-PF Cermet Inserts for Steel, Cast Iron, and Stainless Steel - Finishing","description":"\u003ch3\u003eProcessing Materials\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P)\u003c\/em\u003e\u003c\/strong\u003e - Steels - Alloy Steels\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(M)\u003c\/em\u003e\u003c\/strong\u003e - Stainless Steels (Inox)\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(K)\u003c\/em\u003e\u003c\/strong\u003e - Cast Irons\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eChipbreaker\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(PS)\u003c\/em\u003e\u003c\/strong\u003e - Geometry specially designed for finishing on steels, stainless steels, and cast irons. Features a \u003cstrong\u003esmall rake angle\u003c\/strong\u003e and is available with \u003cstrong\u003esmall cutting radii\u003c\/strong\u003e (\u003cem\u003eRE\u003c\/em\u003e). Suitable for small cutting depths (\u003cem\u003eAp\u003c\/em\u003e) and low feeds (\u003cem\u003eFn\u003c\/em\u003e). Used for cermet grades. Ensures excellent surface quality.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eGrade\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eYT100\u003c\/em\u003e\u003c\/strong\u003e – New generation general-purpose cermet (P10–P20 \/ M10–M20 \/ K10–K20). Increased wear resistance, with a special surface for top finishing.\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eFeed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003eFn\u003c\/em\u003e\u003c\/strong\u003e = 0.06~0.25 mm\/rev\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003ch3\u003eCutting Speed\u003c\/h3\u003e\n\u003cul\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P1-5)\u003c\/em\u003e\u003c\/strong\u003e - Vc=150~480 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P5-9)\u003c\/em\u003e\u003c\/strong\u003e - Vc=160~480 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(P10-11)\u003c\/em\u003e\u003c\/strong\u003e - Vc=70~180 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(M12-13)\u003c\/em\u003e\u003c\/strong\u003e - Vc=120~180 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(M14)\u003c\/em\u003e\u003c\/strong\u003e - Vc=130~260 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(K15-16)\u003c\/em\u003e\u003c\/strong\u003e - Vc=130~450 m\/min\u003c\/li\u003e\n\u003cli\u003e\n\u003cstrong\u003e\u003cem\u003e(K17-18)\u003c\/em\u003e\u003c\/strong\u003e - Vc=100~400 m\/min\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp\u003e\u003cstrong\u003eTurning inserts from YG1\u003c\/strong\u003e, a top cutting tool manufacturer from Korea.\nThe choice of the appropriate insert depends on the \u003cstrong\u003echipbreaker\u003c\/strong\u003e, i.e., the geometry that helps in breaking and removing the chip, as well as the \u003cstrong\u003egrade\u003c\/strong\u003e, which describes the microstructure and coating of the insert and directly affects hardness and fracture toughness. The \u003cstrong\u003ecutting conditions\u003c\/strong\u003e (speed, feed, depth) must be carefully set to achieve maximum tool performance and life.\u003c\/p\u003e","brand":"Yg","offers":[{"title":"0.10~2.0 \/ 0.4 \/ YT100","offer_id":52950533112131,"sku":"DCMT11T304-PF-YT100","price":5.9,"currency_code":"EUR","in_stock":true},{"title":"0.15~2.0 \/ 0.8 \/ YT100","offer_id":52950533144899,"sku":"DCMT11T308-PF-YT100","price":5.9,"currency_code":"EUR","in_stock":true},{"title":"0.08~2.0 \/ 0.2 \/ YT100","offer_id":52950533177667,"sku":"DCMT11T302-PF-YT100","price":5.9,"currency_code":"EUR","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0572\/8396\/9077\/files\/DCMT11T304-PF_YT100_50ff759f-20f9-4db0-a723-0391478d2e46.png?v=1740402425"}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0572\/8396\/9077\/collections\/DC--07_04c7df40-8dbd-4b59-ae55-ea3ac591b32a.jpg?v=1772785158","url":"https:\/\/organametrisis.gr\/en\/collections\/dc-11-inserts\/%cf%87%cf%81%ce%ae%cf%83%ce%b7_superalloys.oembed","provider":"Όργανα Μέτρησης","version":"1.0","type":"link"}